UDK 614.84 Пожарная охрана. Опасность пожара. Пожары
Results of determination of specific electric resistance of the charred remains of drevesnostuzhechny materials (DSM) in the range of thermal influence from 200 to 500 °C are presented in article. Influence of time of thermal influence and extent of heating on value of specific electric resistance of the charred DSM remains is shown.
fire investigation, the seat of fire, wood-shaving materials, method of measurement of electric resistance of the charred remains